SHOUGANG HIERRO PERU S.A.A.
LOADING FACTORES

IRON ORE GRADES
STOWAGE
FACTOR
(ABOUT - W.O.G.)
ANGLE OF REPOSE
BULK DENSITY
DENSITY
SPECIFIC.
GRAVITY
BLAST.FURNACE PELLETS
0.461 M3/MT
28.0 GRADOS
2.30 T/M3
4.98 T/M3
DIRECT REDUCTION PELLETS
0.461 M3/MT
28.0 GRADOS
2.30 T/M3
5.00 T/M3
HIGH GRADE PELLET FEED
0.320 M3/MT
40.0 GRADOS
2.30 T/M3
4.85 T/M3
HIGH GRADE SINTER FEED
0.306 M3/MT
42.0 GRADOS
2.30 T/M3
5.07 T/M3
PELLETS CHIPS
0.325 M3/MT
37.0 GRADOS
3.029 TL/M3
3.073 TM/M3
3077 KG/M3
4.60 Min.
CALIBRATED SINTER FEED
0.425 M3/MT
35.0 GRADOS
3946 KG/M3
5.077